Embodiment 1
[0030] 50kg dyeing machine, 10 imitation leather garments, net weight 25kg:
[0031] Handwork: First wrap the zipper head of the garment with cloth to prevent scratches and other defective products during the dyeing process——Weighing: Prepare the weight according to the volume of the dyeing machine, generally according to 50% of the weight of the cylinder body to prepare the weight of the garment— ——Pre-treatment: Put the handmade garments into the vat, fill the vat with water until half of the vat, and run for 5 minutes——Dyeing: Add steam and add adhesive and dyeing agent when the temperature is evenly raised to 35°C, and the temperature of the dye is raised to 60°C. The holding time is 60 minutes——sample blowing: color matching, OK——dehydration: dehydration by frequency conversion dehydrator, and the dehydration time is set according to the proofing time—drying and semi-drying: the temperature of the dryer is controlled at 50°C, and the moisture regain of semi-drying is 50-6...
Embodiment 2
[0034] 50kg dyeing machine, 10 imitation leather garments, net weight 25kg:
[0035] Handwork: First wrap the zipper head of the garment with cloth to prevent scratches and other defective products during the dyeing process——Weighing: Prepare the weight according to the volume of the dyeing machine, generally according to 50% of the weight of the cylinder body to prepare the weight of the garment— ——Pre-treatment: Put the handmade garments into the vat, fill the vat with water until half of the vat, and run for 5 minutes——Dyeing: Add steam and add adhesive and dyeing agent when the temperature is evenly raised to 35°C, and the temperature of the dye is raised to 60°C. The holding time is 60 minutes——sample blowing: color matching, OK——dehydration: dehydration time is variable—drying and semi-drying: the temperature of the dryer is controlled at 50°C, and the moisture regain of semi-drying is 50-60%——copy Ball: According to the style of the sample clothing, the general distress...
Embodiment 3
[0038] 50kg dyeing machine, 10 imitation leather garments, net weight 25kg:
[0039] Handwork: First wrap the zipper head of the garment with cloth to prevent scratches and other defective products during the dyeing process——Weighing: Prepare the weight according to the volume of the dyeing machine, generally according to 50% of the weight of the cylinder body to prepare the weight of the garment— ——Pre-treatment: Put the handmade garments into the vat, fill the vat with water until half of the vat and run for 5 minutes ——Dyeing: Increase the temperature and add steam evenly. The holding time is 120 minutes——sample blowing: color matching, OK——dehydration: dehydration by frequency conversion dehydrator, set the dehydration time according to the proofing time—drying and semi-drying: the temperature of the dryer is controlled at 50°C, and the moisture regain of drying and semi-drying 50-60% is enough——Ball copying: According to the style of the sample clothing, the general distr...
PUM
 Login to View More
 Login to View More Abstract
Description
Claims
Application Information
 Login to View More
 Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com