A protective coating and environmental protection technology, applied in the direction of anti-corrosion coatings, polyester coatings, coatings, etc., can solve the problems of unstable storage of water-based coatings and complicated production processes, and achieve excellent rheology, good safety, and good working environment Hygienic effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Add 30 parts of linseed oil, 7 parts of 70# Feituo synthetic wax, and 10 parts of petroleum resin into the reaction kettle in sequence, start stirring at a speed of 10~20 rpm, raise the temperature to 100~110 degrees Celsius and wait until it is completely melted. Stirring speed of 30~35 rpm makes it evenly mixed. Turn off the heating and add 14 parts of sulfonate-based preservatives, 10 parts of calcium carbonate, 8 parts of methyl stearate, 9 parts of lithium-based grease, 12 parts of non-drying alkyd resin and 1,000 parts of the total amount under stirring. 2 / 10 naphthenate driers and 2 / 1000 anti-skinning agents. Wait for it to cool down to 40 degrees Celsius and turn off the stirring and discharging.
Embodiment 2
[0017] Add 40 parts of dehydrated castor oil, 7 parts of 62# fully refined paraffin wax, and 6 parts of C5 petroleum resin into the reaction kettle in sequence, start stirring at a speed of 10~20 rpm, and heat up to 100~110 degrees Celsius until completely melted Then mix it evenly at a stirring speed of 30~35 rpm. Turn off the heating and add 12 parts of sulfonate-based preservatives, 10 parts of calcium carbonate, 6 parts of methyl stearate, 9 parts of lithium-based grease, 10 parts of non-drying alkyd resin and 1,000 parts of the total amount under stirring. 2 / 10 naphthenate driers and 2 / 1000 anti-skinning agents. Wait for it to cool down to 40 degrees Celsius and turn off the stirring and discharging.
Embodiment 3
[0019] Add 30 parts of dehydrated castor oil, 10 parts of wax paste with a dropping (melting) point of 75 degrees Celsius, and 4 parts of C5 petroleum resin into the reaction kettle in turn, start stirring at a speed of 10 to 20 rpm, and heat up to 100~110 degrees Celsius until it is completely melted, and then mix it evenly at a stirring speed of 30~35 rpm. Turn off the heating and add 12 parts of sulfonate-based preservatives, 10 parts of calcium carbonate, 6 parts of methyl stearate, 9 parts of lithium-based grease, 10 parts of non-drying alkyd resin and 1,000 parts of the total amount under stirring. 2 / 10 naphthenate driers and 2 / 1000 anti-skinning agents. Wait for it to cool down to 40 degrees Celsius and turn off the stirring and discharging.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com