High-purity and high-density aluminum-titanium alloy ingot and manufacturing method thereof
A technology of aluminum-titanium alloy and manufacturing method, which is applied in the field of high-purity and high-density aluminum-titanium alloy ingots and its manufacturing, can solve the problems of uneven composition, non-dense structure, and high smelting cost of intermediate alloy ingots, and achieve the reduction of gas inclusions, Small molecular diameter, good air permeability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A high-purity and high-density aluminum-titanium alloy ingot, the aluminum-titanium alloy ingot is 15% aluminum-titanium, which contains 83% aluminum, 15.97% titanium and 0.03% impurities.
[0024] The manufacturing method of the above-mentioned high-purity and high-density aluminum-titanium alloy ingot comprises the following steps:
[0025] 1) Raw material preparation
[0026] ① Raw material preparation: Prepare 830Kg of aluminum ingots with a purity of not less than 99.95%, 105Kg of titanium sponge, and 65Kg of recycled waste titanium pins by weight;
[0027] ②Auxiliary material preparation: prepare a sufficient amount of carbon monoxide;
[0028] ③Equipment and tooling preparation: a silicon carbide ceramic hydraulic cylinder with a carbon fiber heating system inside, a silicon carbide ceramic hydraulic rod matched at the input end of the hydraulic cylinder, a silicon carbide ceramic output pipe connected to the output end of the ceramic hydraulic cylinder, and a c...
Embodiment 2
[0037] The whole is consistent with Example 1, the difference is:
[0038] A high-purity and high-density aluminum-titanium alloy ingot, the aluminum-titanium alloy ingot is 15% aluminum-titanium, which contains 85% aluminum, 13.98% titanium, and no more than 0.02% impurities.
[0039] The manufacturing method of the above-mentioned high-purity and high-density aluminum-titanium alloy ingot comprises the following steps:
[0040] 1) Raw material preparation
[0041] ① Raw material preparation: Prepare 850Kg of aluminum ingots with a purity of not less than 99.95%, 95Kg of sponge titanium, and 55Kg of newly purchased titanium pins by weight;
[0042] 2) Metal liquid acquisition and purification
[0043] ①Put the original aluminum ingot prepared in step ① in 1) into the vacuum electroslag remelting equipment prepared in step ③ of stage 1), and put it in a vacuum degree of 10- 4 Heat in the environment of Pa until the aluminum ingot is completely melted, and then continue to h...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com