The invention relates to a preparation method of a 
tissue repair material. The preparation method comprises the following steps: carrying out pre-treatment; vibrating in an 
organic solvent to degrease; deactivating a 
virus with an 
ethanol solution; removing cells by high and low osmotic solutions; swelling in an acidic or alkaline liquid; and quickly lyophilizing and sterilizing. The thickness of the 
tissue repair material is increased by 2-4 times, and the material is loose and porous, small in change of 
mechanical property and degradation property and good in 
cell removal effect and has relatively high 
biosafety and 
biocompatibility. Due to the structural characteristics of proper thickness and looseness and 
porosity, the material is suitable for 
damage repair for filling damaged parts required by repair such as 
cartilage injury, 
skin and 
soft tissue defect, gingival recession and the like. Animal experiments verify that the repaired region after eight weeks has no depressed phenomena and is fully replaced by regenerated tissues. Moreover, the regenerated tissue and 
autologous tissue are healed well and are free of separating phenomenon, which verifies that the material can provide sufficient three-dimensional space for 
cell proliferation and crawl, so that the repaired region has good integration degree and filling degree, thereby realizing 
tissue repair and regeneration.