The present invention provides an anti-aging 
cerium-
zirconium composite oxide. The 
cerium-
zirconium composite oxide has a specific surface area of 80 m<2> / g or more, a pore volume of 0.55-0.80 ml / g, an 
oxygen storage capacity of 500-1200 [mu]mol O2 / g and two-pore group distributed apertures, wherein the 
diameter of the first pore group is concentrated at 3-10 nm, and the 
diameter of the second pore group is concentrated at 15-80 nm. The 
cerium-
zirconium composite oxide provided by the invention has a significant anti-aging activity and a good low-temperature catalytic activity, and can be used for catalyzing hydrocarbons, carbon oxides and / or 
nitrogen oxides in mobile source 
exhaust gas. A preparation method of the cerium-zirconium composite 
oxide, provided by the invention, does not use a surfactant, and reduces 
sewage discharge, so the method is green and 
environmentally friendly; an 
ionic liquid and 
anhydrous ethanol can be recovered by simple 
distillation, so the cost is greatly reduced, and the method is particularly suitable for industrial production; and the composite 
oxide with uniform element 
crystal lattice 
doping distribution and no phase separation is obtained, so the preparation method is of great significance to study mobile source 
exhaust gas treatment purifiers containing the cerium-zirconium composite 
oxide.