The invention provides a method for manufacturing and 
tempering bainite wear-resistant steel and steel 
pipe. The 
bainite wear-resistant steel contains the following main ingredients of: C, Mn, Si, Cr, Ni, Cu, V, Al, P, S and the balance of Fe. The method for manufacturing the 
bainite wear-resistant steel 
pipe comprises the following steps of: alloying the 
raw material ingredients of bainite wear-resistant steel to form an 
alloy, refining the 
alloy by using a refining furnace, forming a 
pipe blank by using 
continuous casting, then, heating up the pipe blank, carrying out heat insulation to homogenize, then, perforating, carrying out tandem rolling, and 
sizing; carrying out pipe-making by using on-line rolling, then, carrying out 
air cooling or accelerated cooling; and after 
air cooling or accelerated cooling, carrying out 
tempering and heat insulation for 1-48 hours at the 
tempering temperature of 180-380 DEG C. Compared with the prior art, the method has the advantages that: the occurrence of mixed-
metal texture is avoided, the recrystallization is fully guaranteed after the 
alloy is homogenized, two difficult problems in composite pipes internationally and domestically are solved, and a pipeline formed by directly adopting the bainite wear-resistant steel pipe is pressure-proof and wear-resistant.