The invention belongs to the technical field of building materials, and provides a novel high-temperature-resistant non-curing waterproof 
coating. The 
coating is composed of the following components in percentage by weight: 25-35% of 
asphalt, 15-30% of rubber oil, 10-20% of waste tire rubber 
powder, 5-10% of 
styrene-butadiene rubber, 1-3% of 
styrene-butadiene-
styrene (SBS), 4-10% of tackifying resin, 10-20% of 
fly ash, 2-5% of a high-temperature modifier and 2-5% of a 
viscosity reducer, wherein the high-temperature modifier is a BL modifier or 
polyamide wax. The preparation method is carried out by adopting a three-section-type feeding method and comprises the following steps: adding 
asphalt and rubber oil, carrying out heating to 150 DEG C, then adding the SBS, the styrene-butadiene rubber, the tackifying resin and the 
viscosity reducer, carrying out heating to 180 DEG C, then adding the 
fly ash and a high-temperature modifier, mixing the components at 180 DEG C to form a uniform liquid, and carrying out cooling and discharging to obtain the novel high-temperature-resistant non-curing waterproof 
coating. The invention solves the problem that a non-curing rubber 
asphalt waterproofcoating is poor in 
heat resistance.