The invention discloses an organosilicone room-temperature-cured anticorrosive 
coating material. The organosilicone room-temperature-cured anticorrosive 
coating material is prepared through mixing the following 
raw material ingredients in parts by weight: 24-40 parts of alpha,
omega-dihydroxyl 
polydimethyl siloxane, 6-10 parts of hydroxy-terminated polyphenylmethyl 
siloxane, 0.5-5 parts of aerosil, 10-30 parts of aluminum 
hydroxide powder, 0.5-5 parts of nano 
calcium carbonate, 5-15 parts of 
pigment slurry, 5-9 parts of cross-linking agent, 1-2 parts of 
coupling agent, 0.1-1 part of catalyst, 1-2 parts of modified 
polytetrafluoroethylene powder and 5-10 parts of 
thinning agent. According to the 
coating material disclosed by the invention, coating 
layers can form uniform and fine paint films, are very good in flexibility and are free of 
erosion resulting from harsh climate environments and corrosive medium environments; the coating material disclosed by the invention is cured at 
room temperature, is simple in construction, is directly coated, can be subjected to 
brush coating and roller coating and can also be subjected to 
spray coating; the adhesion of the paint films reaches the level 1; the paint films are waterproof and dustproof; the 
impact resistance is excellent; and the heat and 
weather resistance and 
flame retardance are also very excellent.