The invention relates to a 
rare earth ore 
beneficiation method which is characterized in that grading is carried out after ore 
grinding is carried out on raw ore; reselection is carried out on coarse fractions to obtain gravity concentrates and 
tailings; 
magnetic separation is carried out on fine fractions to obtain strong-
magnetic separation concentrates and 
tailings; reselection is respectively carried out on gravity concentrates and strong-
magnetic separation concentrates which are different in fraction through a table to obtain table concentrates, table middlings and table 
tailings; the table concentrates and the table middlings which are different in fraction are mixed, and wet-type high-gradient magnetic separation is carried out to obtain magnetic separation 
rare earth ore concentrates and magnetic separation middlings; the magnetic separation middlings and the table tailings are mixed, closed-loop flotation including primary rough concentration, secondary 
scavenging and secondary fine selection is carried out after ore regrinding is carried out, the middlings are returned in proper sequence, and flotation 
rare earth ore concentrates and flotation tailings are obtained. The magnetic separation rare earth ore concentrates and the flotation rare earth ore concentrates are total rare earth ore concentrates, the REO grade is higher than 65%, and the 
total recovery rate ranges from 80% to 87%. The rare earth ore 
beneficiation method is high in grading efficiency, small in occupied area, continuous in production and low in cost, full-wet dust-free operation is achieved, and industrialization is easy to achieve. The rare earth ore 
beneficiation method is suitable for beneficiation of light rare earth ore existing in the bastnaesite or parisite mode.